{Experiment.Sample}
Material_Name: Platinum doped Permalloy
Form: ~20nm film on Si wafer

{Experiment.Measurement}
Detection: total electron yield
Temperature: RT
Orientation: 30° grazing incidence
Date: 2015-06-24
Measured_by: Alpha T. N'Diaye

{Ni20Fe80Pt10}
Ni_XMCD.get_xmcd.energy_range: 800 1000
Fe_XMCD.get_xmcd.energy_range: 600 800

{Ni20Fe80Pt10.Ni_XMCD.xas_normalization_to_min_and_max}
energy_range: 800 1000
normalization_factor: 0.952002315041
offset: 0.358620768783

[+Ni20Fe80Pt10.Ni_XMCD_Spectra]
Energy,XAS,XMCD
820,0.0104944,-0.00140602
821,0.0104183,-0.000451802
822,0.00931404,-0.000974055
823,0.00821621,-0.00083305

[+Ni20Fe80Pt10.Fe_XMCD_Spectra]
Energy,XAS,XMCD
680,0.0670848,0.000905727
681,0.0659347,-0.00085033
682,0.0631599,-8.87504e-05
683,0.0591931,-0.00278828

[+Ni20Fe80Pt20]
# bare data section, i.e. identifier and CSV table
Energy,XAS,XMCD
680,0.0670848,0.000905727
681,0.0659347,-0.00085033
682,0.0631599,-8.87504e-05
683,0.0591931,-0.00278828